TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Victor Hernandez <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 6 Jul 2010 06:47:12 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (51 lines)
How does the SJ look like in x-ray?

"X"

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ashok Dhawan
Sent: Monday, July 05, 2010 11:02 AM
To: [log in to unmask]
Subject: [TN] QFN : what is minimum solder thickness to rework

I am debating on what is minimum acceptable solder joint thickness for QFN-32 
packages ? Just for clarity , QFN-32 is bottom termination part with no toe 
joint due to exposed copper on toe. 

We did cross sectioning and found that solder thickness varies form 15 microns 
to 45 microns - different footprints. We are wondering what should be minimum 
acceptable thickness before we need to rework ?  Any graph or relationship to 
determine reliability of joint with respect to thickness of joint ? 

We are building Class3 products for automotive industry. No information found 
on thickness of solder joint Except for IPC-7093 (unreleased draft copy) where 
the solder thickness is mentioned as 50 microns. 

Anybody to share what should be used as minimum thickness before 
reworking ? 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2