Ian,
I would agree with Graham has said. Our experiences are about the same.
To Graham's 3 suggestions I would add a fourth. You can possibly use an
elastomeric sealant around the outside of the BGA to seal off the inside.
This works well especially if you are going to conformally coat the
opposite side of the board for any access vias.
Doug Pauls
Graham Collins
<Graham.Collins@L
-3COM.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
07/20/2005 05:49 Re: [TN] Coating under BGA's
AM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Graham Collins
<Graham.Collins@L
-3COM.COM>
Hi Ian
In our applications we have used one of three options depending on what
the product is and where it is going:
1) underfill the BGA with a purpose made material, not with conformal
coating.
2) parylene coat the assembly (which, by virtue of it being a vacuum
deposition process, will coat under the BGA)
3) spray coating on the board and accept that the BGA underside is
shadowed.
#3 isn't without precedent, we don't typically worry much about old
style boards with pin grid array components...
I would not underfill a BGA with a regular coating material. This has
been discussed in the past on TechNet, one of the concerns is the
expansion with temperature putting stress on the joints.
Good luck!
regards,
Graham Collins
Process Engineer,
L-3 Communications Electronic Systems Inc.
Halifax
(902) 873-2000 ext 6215
>>> [log in to unmask] 07/19/05 01:23PM >>>
Fellow techies, a BGA related question. We're just starting to design
BGA's
into some new designs which are class 3 high rel assemblies and I am
asking
myself questions about the ability to adequately conformally coat under
the
packages. Our standard coating is a solvent based acrylic and we are
using a
456PBGA device and a 429CBGA device, both on 1.27mm pitch, as the
maximum
sizes so far and I'd be interested to hear what other class 3 builders
have
experienced when applying the coating.
Regards
Ian Fox
Goodrich ECS
Birmingham
UK
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|