TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Macconnell, Richard (ES)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Macconnell, Richard (ES)
Date:
Mon, 25 Sep 2006 09:57:56 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (94 lines)
Richard:

You are correct.  I had it reversed.  The Sn96 comes first.

Too close to the weekend, I guess.  

Rich. 

-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]] 
Sent: Monday, September 25, 2006 5:35 AM
To: TechNet E-Mail Forum; Macconnell, Richard (ES)
Subject: RE: [TN] Soldering with Sn9,5Ag3,5

This does not make sense. Sn96 has a higher melting temperature than Sn63. Do you mean this the other way around? What process are you describing? 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Macconnell, Richard (ES)
Sent: Friday, September 22, 2006 10:32 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering with Sn9,5Ag3,5

Arnaud:

We use Sn96 (referred to as high-temp solder) in processes where there are two soldering operations.  Sn63 solder is used in the first operation, followed by the Sn96 in the second.  This avoids reflowing the Sn63 during the second soldering.

I don't know enough about soldering to be able to answer Juan's question.  But, if the intent is to solder the tinned wires to the board, isn't some melting of the SnPb coating on the board required?  If so, why use a high-temp solder?  Switching to ENIG gets around that issue.

Rich. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of arnaud grivon
Sent: Friday, September 22, 2006 6:20 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering with Sn9,5Ag3,5

Could anybody on the TechNet planet tell me the primarily reasons for using this Sn96,5Ag3,5 solder alloy?
It looks like this alloy has been already in use for some years as solder wires and solder paste for small electronic modules.
Also, I seem to remind that this was the first alloy of choice for lead-free BGA spheres before the industry consensus for SAC.
Why did the industry switch to SAC instead of SnAg? In other words, what does the copper bring?

A. Grivon

Juan T. Marugán a écrit :
> Hi,
>
> in a Class 3 product (aerospace) we have to solder some wires to a PCB 
> using a Sn96,5Ag3,5 solder alloy. Wires are silver coated, 
> high-strength copper alloy and the PCB is SnPb plated.
>
> My first question is, Do you consider that solder alloy as a good option?
>
> Besides, in a near future, we will change the finish of the PCB from 
> SnPb to ENIG. In that situation, what solder alloy do you recommend us?
>
> Thank you in advance.
>
> Juan T. Marugán
> Production QA
> Indra Sistemas SA
> Spain
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>   

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2