Gee, I haven't heard of GEE material before, but you're right, the third
character is generally a color designation, although it's listed in
MIL-S-13949 as "Special Consideration".
GE is G-10 (non-brominated, hence non-flame retardant, epoxy), while GF is
(brominated) FR-4.
Timothy Reeves
QA Manager/Process Engineer
ECD Circuit Board Division
|-----Original Message-----
|From: Stephen R. Gregory [mailto:[log in to unmask]]
|Sent: Wednesday, September 20, 2000 10:01 AM
|Subject: Mil laminate designations...
|
|
|Hi all!!
|
|What does the last "E" in the Mil designation type "GEE"
|laminate stand for?
|I though it was the color...for instance "GEN" would be a G-10
|natural color,
|right?
|
|Also, is there any real difference in "GE" vs. "GF" laminate material?
|
|Thanks!
|
|-Steve Gregory-
|
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|