We use
Peelable mask
Selective wave carriers
And a long time ago we used a passivated Ni (or NiSn????) finish
Regards
Rex
Rex Waygood
Technical Manager
Hansatech EMS provides value manufacturing through engineering and quality
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY
+44 (0)1202 338200
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of henry rekers
Sent: 02 December 2009 00:28
To: [log in to unmask]
Subject: [TN] Pad that does not solder.
Hi,
I have an application where I need to force a pad to not solder (or at least solder to a consistent thickness) in wave solder. The pad will eventually recieve a mechanical connection. I'm trying to design a land that will either skip, or solder to a consistent minimum thickness. The pad is large about 0.500 by 0.500. Maybe some sort of a checkerboard, or grid of vias, etc? The wave is leadfree with sac solder.
Selective soldering has already been ruled out due to other design constraints, and I'm also pursuing the idea of peelable mask.
Any ideas?
Thanks.
Henry.
__________________________________________________________________
Make your browsing faster, safer, and easier with the new Internet Explorer® 8. Optimized for Yahoo! Get it Now for Free! at http://downloads.yahoo.com/ca/internetexplorer/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|