TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 21 Jun 2005 10:53:59 -0700
Reply-To:
Subject:
From:
Gene Felder <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
Desco
MIME-Version:
1.0
Parts/Attachments:
text/plain (127 lines)
VPI recently discontinued its "Glaze" product, but a number of companies
have Dissipative Floor Finishes to transform most any hard floor into an
ESD Floor.  Periodic re-application is required.

Per ESD Handbook TR20.20 section 5.3.4.2 Functions of Static Protective
Floor Materials
"Floor finishes and topical antistats, on the other hand, function by two
separate mechanisms. First, they reduce the surface's tendency to generate
a static charge. Second, they provide a path for the dissipation of charge.
The charge may dissipate over the surface of the finish or it may dissipate
to ground if the floor finish is grounded."

Per section 5.3.4.7.8 Floor Finishes "Static-limiting floor finishes are
applied to a variety of existing floors--standard
vinyl, rubber, or vinyl composition tile, or static control flooring--to
reduce the generation of electrostatic charges. As a floor finish, they
protect and they improve the appearance of the floor, and make floor
maintenance easier. Floor finishes have flexibility of use, can be applied
throughout a facility, and can provide whole area protection.

These materials also have some disadvantages. Some surfactant type finishes
may become too slippery. Some finishes are subject to being washed off with
ordinary water. Some finishes can be worn away readily. They require
additional monitoring to make sure that the finish is still working.
Improper application and maintenance may cause inconsistent performance of
the finish. Some floor finishes may be incompatible with clean room
requirements."

Regarding the "too slippery" comment, some products are UL listed regarding
slip resistance.

Gene Felder
[log in to unmask]

-----Original Message-----
From:   Lee Whiteman [SMTP:[log in to unmask]]
Sent:   Tuesday, June 21, 2005 10:12 AM
To:     [log in to unmask]
Subject:        Re: [TN] ESD flooring

Bob,

What ever you do to that floor, DON'T WAX IT!

I have an emotional response to you query. In a previous life, we
installed an ESD floor and it worked perfectly until a maintenance man
one evening waxed it, destroying about 10,000 sq. ft. of ESD floor
tiles.

Now there may be a floor wax which will not damage the ESD floor tile. I
would recommend that you contact the ESD floor tile's manufacturer to
determine what materials to use to clean the floor. You will ruin the
properties of the floor if you do not follow the maintenance procedures.

Hope this helps.

Good Luck.

Lee Whiteman
Senior Manufacturing Engineer
American Competitiveness Institute
E-Mail: [log in to unmask]
Ph: (610) 362-1200 x208
Fax: (610) 362-1290

This message is for informational purposes only and does not supersede,
modify, or create any agreements with ACI. Information contained in this
message does not bind ACI or its affiliates to any commitment, either
express or implied, unless ratified in writing by an authorized
representative.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Arciolla
Sent: Tuesday, June 21, 2005 11:43 AM
To: [log in to unmask]
Subject: [TN] ESD flooring


Good Morning All,

I have a question regarding ESD flooring. Does flooring tile have to be
ESD tile or can you just wax over  tile with ESD wax?

Thanks,

Bob Arciolla
Endicott Research Group

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Quality/Safety Manager

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2