text/plain (32 lines)
A word of warning about "Galvanic Metal Charts"

They are almost useless in the real world, and actually only report on
oxidation values in pure water....and what else is present (the electrolyte)
makes ALL the difference.

Example....one metal will immersion plate on another when the metal in
solution is more electronegative than the substrate....i.e. metals below a
given metal should be able to plate on to metals above on the usual charts.

Yet, depending on the electrolyte, you can make Tin immersion plate on to
Copper, OR Copper immersion plate on to Tin...

So, their relative postions on the Galvanic metal chart are wholly dependent
on the electrolytes present...

Life is NEVER simple...

Rudy Sedlak
RD Chemical Company

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2