There should be no need to clean the assemblies after fluxing with the NR200, if the soldering process is under control and validated.
Both Alpha and Kester have provided me with great technical support. My suggestion would be to contact the manufactures of the fluxes.
SCOTT
-----Original Message-----
From: Charles Caswell [SMTP:[log in to unmask]]
Sent: Thursday, September 20, 2001 9:34 AM
To: [log in to unmask]
Subject: Re: [TN] Mixing fluxes
If the subcontractor ( your company ) is cleaning the assembly after
soldering you will not be mixing flux. There should be no NR200 left on
the boards.
Charles Caswell
Process Lead, PCB
Frontier Electronic Systems
-----Original Message-----
From: TechNet E-Mail Forum. [mailto:[log in to unmask]]
Sent: Thursday, September 20, 2001 9:49 AM
To: [log in to unmask]
Subject: [TN] Mixing fluxes
Does anyone know of any data concerning mixing fluxes, specifically
Kester
965 and Alpha NR200. Our
situation is that we use Kester 965 in our wave solder and rework
process.
We have some boards
being built by a subcontractor using Alpha NR200. Can we rework these
boards safely with Kester 965 flux?
Thanks!
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|