TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"BILL RUGG" <[log in to unmask]>
Date:
Wed, 29 May 96 09:05:00 MDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (23 lines)

Comments :

------------------------[ Original Message ]--------------------
To		: ISMTP@Longmont64@MCO[[log in to unmask]]
Cc		: 
From		: BILL RUGG@ENG12@MCO
Date		: Tuesday, May 28, 1996 at 2:13:05 pm MDT

 - Hi

 I am trying to establish a PCBA flexure force level for compression 
connectors.  The compression connector and mating PCB surface is tin lead. 
The measured contact force per contact range from 170 to 280 grams. The 
force generated a 0.57% Bow and Twist after soldering which has some 
margin below the ANSI/J-STD-001 9.2.3 of 0.75% for SMT boards. Does anyone 
know of a solder joint or a assembled component stress guideline other 
than the J-STD-001 Bow and Twist Specification.

			Thanks,	Bill