Folks, I reply only to say that I always followed John's instructions
concerning the cause of MLCC cracks, and his articles are one of my holy
books.
Everybody can read , understand and improve the so wide spread occurrence of
mechanical cracks if he checks his articles in the AVX technical papers.
Just looking at the position of the capacitor near the connector, you can
see that being the only one which cracks has to do with mechanical stress.
When, how, where, is the challenging investigation everybody has to do on
his own, as there are no identical circuits, processes and strains.
But again, placing the ceramic capacitor near a connector pin means trouble,
and it comes AFTER reflow soldering.
These days, there are lots of articles on this matter written by specialists
from many companies which manufacture MLCC's and research institutes, all in
accordance with his older articles but the best I found is:
www.calce.umd.edu/whats_new/2001/design.pdf
And don't forget that not all MLCC's are able to withstand the same bending
forces- their data sheets contain this parameter.
Thank you John for being there and giving your knowledge so freely!
Gaby
----- Original Message -----
From: "Brian Chandler" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, April 29, 2008 3:02 PM
Subject: Re: [TN] Cracking Ceramic Cap
Have you tried to take any strain measurements during the processing
downstream of SMT? ICT fixtures can induce excessive strain as well as any
other fixturing/pallets.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|