TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Date:
Wed, 17 Jun 2009 15:24:02 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Tony Steinke <[log in to unmask]>
Subject:
From:
Tony Steinke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="windows-1250"
MIME-Version:
1.0
Parts/Attachments:
text/plain (157 lines)
Steve,
The dryfilm soldermask as tenting is old technology. I am surprised your pad
height is not greater than .003. Lackwerke Peters, DuPont and several others
make a tenting paste that eliminates pad height problems but still gives you
a tented hole. Your supplier may not be aware/experienced with the process.

Tony Steinke

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Wednesday, June 17, 2009 12:45 PM
To: [log in to unmask]
Subject: Re: [TN] SolderMask Question

This is known as tenting. Usually the final height will be below 0.003,
but no one will want to be held to that limit. If there is a functional
reason you are incorporating a via protection strategy, then there are
only 3 accepted scenarios that will pass a Class 3 or 3/A requirement
for long term reliability in an Aerospace or high-rel environment. Their
descriptions can be found in IPC-4761 and the 3 types are as follows:

*         Type II-b

*         Type VI-b

*         Type VII

 

Dewey

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vargas, Stephen M
Sent: Wednesday, June 17, 2009 9:22 AM
To: [log in to unmask]
Subject: [TN] SolderMask Question

 

All:

 

 

 

We have a Class III PCB, that we are building using leaded technology

(non-RoHS), HASL finish, where my customer is specifying double masking

over vias for "via protection". Dry film is initially being placed over

the vias only, then the board is covered by LPI. Our problem is that it

creates problems with the solder stencil not properly gasketing to the

PCB during screen-printing resulting in solder defects. We are seeing

raised solder mask as high as .003". Is this (double masking)

commonplace? Are there more "manufacturing friendly" options for optimum

via protection? I've asked about possibly using dry film mask only (no

LPI on top), but was told that the mask feature sizes are too small for

dry film. Any insight would be appreciated. 

 

 

 

Regards,

 

Steve Vargas

 

 

 

Polaris Contract Mfg Inc

 

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:
http://listserv.ipc.org/archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

Internal Virus Database is out-of-date.
Checked by AVG. 
Version: 7.5.560 / Virus Database: 270.12.36/2126 - Release Date: 5/21/2009
6:22 AM
 

Internal Virus Database is out-of-date.
Checked by AVG. 
Version: 7.5.560 / Virus Database: 270.12.36/2126 - Release Date: 5/21/2009
6:22 AM
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2