Hello Technet team,
We have a laminate based QFN package with ENIG plating on terminations. Using lead based paste Sn63/Pb37, we fail solderability test per JESD22B102E (dip and Look test) and also per J-STD-002 method B (dip and Look test). However, we passed reflow solderability test using lead free paste (SAC 305) per method JESD22B102E . Due to product requirements, we have to use eutectic Sn63/Pb37 solder paste. The reflow oven is convection air . If anyone had this issue and can share some insight or inputs will be much appreciated.
Thank-you,
Mumtaz
858-795-0112
CONFIDENTIALITY NOTE: The information transmitted, including attachments, is intended only for the person(s) or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and destroy any copies of this information.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|