Jim,
We have seen it in GIL-style Polyamide. There are filler materials that are
put into the "fill" area where the copper was removed. The process was used
a lot when CIC is used with polyamide base material. The prepreg flows and
coated the material, and the filler makes the 'filled' area less brittle.
I have only bought boards like this. Personally never built boards using
it. Don't know the parameters. The filler material might be a Ceramic.
May not work in Cyanide. I can't think of any other disclaimers. Good
Luck!
George Franck
Raytheon Systems
Falls Church Virginia
"My Opinions are just that."
----------
From: James A Larson <[log in to unmask]>
To: [log in to unmask]
Subject: [TN] Radial Cracks on Cyanide Ester resin
Date: Mon, 8 Jun 1998 15:42:01 +0100
Has anybody experienced Radial Cracking as viewed from a
horizontal section or Fishscale cracking as viewed from a
vertical section using Cyanate Ester Resin. This resin system
is used to fill a 2 oz. copper plane layer in a 8 and 10 layer board.
If so what parameters have you compensated for to help
minimize this situation?
We've modified press parameters and drill parameters with
minimal success.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|