TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-mail Forum <[log in to unmask]>
Date:
Mon, 15 Jun 2009 10:47:51 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bill Dworak <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Bill Dworak <[log in to unmask]>
Parts/Attachments:
text/plain (18 lines)
Hello everybody, I am looking for some knowledge on what I see is a basic type problem that is driving me crazy. I am a sales guy who covers a sizable territory and in that territory for a PCB manufacturer (yes one of those) I have one account that I have been working with for about 4 years now that continuously has issues assembling both hand assembly as well as pick & place. 
The surface finish is HAL (leaded) this is a military account that is pretty well structured in their processes. What I get told is that there seems like a contamination is on the surface when they scrub the surface it makes it better but not 100% better.They have sent back samples for us to look at , we saw nothing on the surface no contamination nothing wrong at all. 
If this was one of a few that has the same or similar issues it would make some sense and I could go to the people I work with asking them to look into this issue. But it is the only company that has this issue. 
 Has anybody seen a similar type of a situation before? Understood that you cannot fix this but would appreciate advise as to where to look so hopefully this can be solved. 
Thank you. 

 Bill Dworak 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2