TECHNET Archives

October 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ed Popielarski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ed Popielarski <[log in to unmask]>
Date:
Tue, 18 Oct 2016 14:48:35 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
http://www.upa.com/microderm.php





Ed Popielarski

Engineering Manager





                               970 NE 21st Ct.

                              Oak Harbor, Wa. 98277



                              Ph: 360-675-1322

                              Fx: 206-624-0695

                              Cl: 360-544-2289







       “It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”

https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Wettermann

Sent: Tuesday, October 18, 2016 7:01 AM

To: [log in to unmask]

Subject: Re: [TN] Measuring Gold Thickness



Gents/Ladies:



This would be confirming gold plating thickness after repair using a brush plating technique. Repair thickness is a function of many variables....



I was looking for an instrument to verify that would be cost effective as it is for this single use.





Bob/BEST



On Tue, Oct 18, 2016 at 8:37 AM, Bev Christian <[log in to unmask]>

wrote:



> XRF

>

> Bev

>

> Sent from my BlackBerry 10 smartphone on the Bell network.

>   Original Message

> From: Bob Wettermann

> Sent: Tuesday, October 18, 2016 9:28 AM

> To: [log in to unmask]

> Reply To: TechNet E-Mail Forum

> Subject: [TN] Measuring Gold Thickness

>

> Outside of x-sectional measurements for QA. can someone please share 

> their favorite method/instrument for measuring gold thicknesses on PCBs?

>

> Thanks

>

> Bob/BEST

>







--