TECHNET Archives

June 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Wed, 4 Jun 2014 09:02:02 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Larry Dzaugis <[log in to unmask]>
Subject:
From:
Larry Dzaugis <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (22 lines)
The peelable may work.
You have to test it first. Some may lift on the edge and be washed off.
Technique may require refinement.
Depends what is being protected.
The mask may or may not seal a component against the wash water.
Variables included surface adhesion, impingement force and angle,
wavesolder operation, method of application.

The water soluble works.
Pay attention to the dry time.
Too little and it washes off in wave.
Too long (day or two) it dries out and cracks.
Both results in solder where it shouldn't be.

Even the peelable can have a problem with too short a time.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2