Greg,
AlphaLEVEL is a silver immersion process used as an alternative to HASL.
For additional information please contact Steve Beigle:
[log in to unmask] off-line.
Regards,
Eric Yakobson
Alpha PC Fab
Greg Way <[log in to unmask]> on 08/06/98 05:11:00 PM
To: [log in to unmask]
cc: (bcc: Eric Yakobson/AlphaPCFabUS/Cookson)
Subject: [TN] Alpha Leveling
I am looking for information regarding the alpha leveling process used for
depositing solder on blank pcb's prior to board stuffing. In particular,
what particular pitfalls there may be for new players, and also who may be
contacted to source boards (FR4) tinned using this process
Greg
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|