thanks! Werner
The ball material of the BGA is SAC-305.
Which should I choose to use as paste for high reliability between
SAC305,SAC405,SAC105,and leaded tin?
hechong
Werner engelmaier <[log in to unmask]>
发件人: TechNet <[log in to unmask]>
2008-12-09 07:28
请答复 给
TechNet E-Mail Forum <[log in to unmask]>; 请答复 给
Werner engelmaier <[log in to unmask]>
收件人
[log in to unmask]
抄送
主题
Re: [TN] ??: Re: [TN] BGA soldering open issue
Hi Victor,
Normally these pics open--now I am on the road and things get even more
difficult.
It is not the weight but the different thermal expansion of the various
BGA ayers.
Werner
-----Original Message-----
From: [log in to unmask]
To: [log in to unmask]
Cc: [log in to unmask]
Sent: Sun, 7 Dec 2008 1:29 pm
Subject: RE: [TN] ??: Re: [TN] BGA soldering open issue
Werner,
?
?? I was unable to open the
file.? ?I can see the borders.? ?I too was not aware that
attached H/S could cause solder bump open issues. ??What is the least
recommended H/S weight that would not cause a BGA solder bump issues?
??Can
you share supporting data/documentation/case study?
?
Victor,
?
From:
[log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, December 05, 2008
3:37 PM
To: Hernandez, Victor G; [log in to unmask]
Subject: Re: [TN] ??: Re: [TN] BGA
soldering open issue
?
Hi Victor,
Here it is:
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
|
|
|