Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (39 lines)
Neil,

  I tent vias to help prevent shorts.

  If a PCB is disposed towards growing dendrites then I would think there is
a serious cleaning problem. 

Bob

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Neil Atkinson
Sent: Wednesday, July 04, 2012 12:02 PM
To: [log in to unmask]
Subject: [TN] Copper Dendrites

 

 What is the view of covering vias with solder resist to prevent dendrite
growth?

This is an FR4 PCB with OSP finish, SMT reflow both sides and a few through
hole components soldered with a selective soldering process...

Thanks in anticipation of the help of the Technet!

Neil


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2