We do this routinely. The thermal shock of a preheated part going
through 500 deg. solder is probably less than touching the part with a
700 deg. iron.
Charles Caswell
Process Lead, PCB
Frontier Electronic Systems

-----Original Message-----
From: Jorge Rodriguez [mailto:[log in to unmask]]
Sent: Tuesday, October 02, 2001 12:29 PM
To: [log in to unmask]
Subject: [TN] Tantalum Caps


Technetters,

I have a product that has Tantalum Caps, having them waved would make
our
life easier, the board has some TH components we currently hand solder
and
that could be waved. I know that there might be some reason not to wave
Tantalums, but I am not sure. Can Tantalum Caps be wave soldered?, Has
anyone done this?

Any responses would be appreciated

Jorge Rodriguez
Process Engineer
Varian Inc

------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2