TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Wed, 16 Jan 2008 19:28:07 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (226 lines)
I'm going to have to think about your response before replying, Vlad. 
Bev

----- Original Message -----
From: Igoshev, Vladimir <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>; Bev Christian
Sent: Wed Jan 16 19:12:07 2008
Subject: Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic

Bev,

The bulk concentration (particularly when you are talking about a ball, not a joint) means almost nothing.

It is important whether the platelets are segregated at the ball surface or they are in the bulk.

Coming back to your original question, I'd have to say that all the answers you've got so far are right to some extent, but all of them should have started withqq a famous phrase "it depends" :-)

In addition, I think you should have asked whether a mixture/alloy of Sn and AuSn4 intermetallics is sokderable.

Let me explain.

If you try to solder to a surface covered with a Sn/ AuSn4 mixture (and the bulk concentration of Au in the mixture/alloy is less than 30%), then you have pure Sn in the mixture and the lower the bulk percentage of Au, the more pure Sn you have in the alloy. IF there is no segregation of the AuSn4 intermetallics at the surface, then the more pure Sn - the easier to solder to it. However, it the intermetallics is segregated at the free surface, then one would be trying to solder to it and according to the Werner's e-mail, it's a bad idea.

Regards,

Vladimir

----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Wed Jan 16 17:24:52 2008
Subject: Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic

Dave,
I only have 0.8 to 1.2% gold in the solder balls - as determined by XRF.
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, January 16, 2008 5:06 PM
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic

Hi gang! Steve - I just sent you another set of photos showing a solder
joint that has gold embrittlement. Bev - if you have a solder joint that
contains the AuSn4 microstructure phase then you have an indication that
your overall composition has exceeded the "magical" 4% limit.  The
presence of the AuSn4 platelets cause the solder joint to behave in a
brittle manner when subjected to some use environments. The formation of
the AuSn4 phase isn't going to interfere with the formation of your solder
joint but they do result in solder joint integrity degradation. The
pretinning of gold plated component leads is an attempt to replace the
gold with a solder coating and lower the overall total percentage of gold
that would exist in the solder joint - the lower the overall solder joint
gold content, the lower the likelihood for the AuSn4 phase to form.

Dave Hillman
Rockwell Collins
[log in to unmask]




Steve Gregory <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/16/2008 03:35 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Steve Gregory <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic






Hi Inge ol' pal!

I went back and looked on my pages, and am not sure if they're still
there. But one of these might be:

http://stevezeva.homestead.com/files/fracture_bad.jpg

http://stevezeva.homestead.com/files/fracture_bad_2.jpg


Steve




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Wednesday, January 16, 2008 3:09 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic

Not really true, the Scottish blood in my veines tells me to be careful
with money, the kyrgise blood makes me crush the table, therefore, noone
can actually be under it.

I think there are pictures from my large AuSn platelets somewhere on
Gregory's wall. If not, I can probably dig them up again from some old
report. If such crystals are abundant in a solder joint, the components
may just jump off the board when giving a mechanical shock.

/Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier /*
Skickat: den 16 januari 2008 20:30
Till: [log in to unmask]
Ämne: Re: [TN] SV: [TN] Solderability of Tin-Gold Intermetallic

Hi Inge,
As usual people are well advised not to argue with a (this) Swede; 1) he
usually knows what he is talking about, and 2) if not, he will drink you
under the table.
The IMCs formed by Sn/Pb, and Sn/Ag as well, are platellet-shaped crystals
(in cross-section they may look like needles but are always plateletts),
and I have seen no evidence that they are solderable. Solderability simply
depends on how much Sn, or SnPb, to which you wet, is present. So the
amount of these IMCs affect both solderability as well as
Au/Ag-embrittlement.
Inge, how is Gerd? I sure have not heard anything about him for some time.



Werner



**************
Start the year off right.  Easy ways to stay in shape.

http://body.aol.com/fitness/winter-exercise?NCID=aolcmp00300000002489

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts:
send e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------





---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2