TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0uWAHh-0000C9C; Tue, 18 Jun 96 18:34 CDT
Encoding:
8 Text
Old-Return-Path:
Date:
Tue, 18 Jun 96 16:22:28 PST
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/4738
From [log in to unmask] Tue Jun 18 20:
10:12 1996
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"imnb82.0.SU7.mppnn"@ipc>
Subject:
From:
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (11 lines)
     
     Anyone pre-baking prior to the wave with OSP on the boards.  Time and 
     Temp?  Seems I heard about an oxidation of the Cu under the OSP, or 
     was the T & T too much?  Question comes up because of the necessity to 
     bake things such as Thermount boards prior to any temp. stressing.  
     
     Thanks, Neal Preimesberger, HMSC Tucson.  520-794-1030