Connie,

Can you cut the lead off and wrap and solder a smaller guage rework wire
to the lead and then to the IC pad/lead?  This will require you to bond
the part to the board, if you weren't already doing so.

Jim Carlson
Rockwell Collins Quality/Reliability Engineer




Connie Korth <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/13/2004 01:03 PM
Please respond to "[log in to unmask]"


        To:     [log in to unmask]
        cc:
        Subject:        [TN] IPC 610 Interpretation


        Good afternoon all,

        We have a rework situation in our facility.  Here goes:

        We have a gull wing component that we have to add a large
through-hole
capacitor lead on to one of the IC leads.  Per the 610 requirement,
12.2.5.5, solder may not touch the body of the component of a gull wing
component.  Because this is not a normal build situation, is that a
requirement that has to be met?  It is very difficult to solder this large
lead on to this small lead, making a solid connection, without getting
solder between the lead and body of the IC.  I realize the 610 is a
guideline for us to make decisions.

        So.........  In your opinion, what would you do?  Rework, accept
as is,
.....
        I realize the final decision is between us and our customer, but
would
like    to hear what others think aobut this.


        Thanks,

        Connie M. Korth
        Quality Specialist
        Reptron Mfg. Services
        [log in to unmask]
        218-262-8209

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-509-9700 ext.5315
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2