TECHNET Archives

February 2019

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
FTL Quality <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, FTL Quality <[log in to unmask]>
Date:
Thu, 7 Feb 2019 15:19:15 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (81 lines)
Are these boards laminated at all? If so is it possible that these are an 
imprint from the lamination press?

-----Original Message----- 
From: Tom Brendlinger
Sent: Thursday, February 7, 2019 3:07 PM
To: [log in to unmask]
Subject: Re: [TN] "Wrinkle" on outer copper layer

Unfortunately I don't have XRF capability in house. I'm hoping to get
approval to send it out.

Interesting theory Steve. The only thing about that theory that I don't
understand is why it would be in the same location on two boards, but not
on the rest. It's possible that it was just luck, but it isn't a super
satisfying answer. I'll see what analysis I can get approved and if it
supports that theory.

Thank you!
Tom

On Thu, Feb 7, 2019 at 7:51 AM Steve Herring <[log in to unmask]>
wrote:

> Is it possible there was a glass fiber on that area when it was plated,
> leaving you with the original copper foil thickness?
> The fiber was then removed prior to ENIG?
>
> My guess at the cause.
>
> Steven E Herring
> Director of Engineering
> Pennatronics Corp
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of FTL Quality
> Sent: Thursday, February 07, 2019 3:07 AM
> To: [log in to unmask]
> Subject: Re: [TN] "Wrinkle" on outer copper layer
>
> Are you able to complete an XRF analysis on the Nickel thickness of the
> ENIG?
>
> -----Original Message-----
> From: Tom Brendlinger
> Sent: Wednesday, February 6, 2019 8:36 PM
> To: [log in to unmask]
> Subject: [TN] "Wrinkle" on outer copper layer
>
> Hello TechNet,
>
> I've recently received some boards that have a defect I've never seen
> before.
>
> There is a linear depression in a 2oz outer copper layer on two out of 45
> boards. One of the boards was on a solder sample panel, the other was
> assembled with the defect.
>
> The depression has the appearance of a wrinkle or groove, it is
> approximately straight and square to the edge of the board. At its widest
> point it is about 0.006" wide, and as far as we can measure it is between
> 0.0015" and 0.002" deep. There are a couple of small delaminations nearby
> (on a panel that has not been reflowed).
>
> I looked through IPC-A-600 and did not find anything about this type of
> issue. I don't have the equipment to microsection or x-ray the board, so
> I'm not sure whether the foil is damaged under the plating (Which is RoHS
> ENIG).
>
> Hopefully this image link works:
> https://snag.gy/Kx58Oy.jpg
>
> Please let me know if you've seen this before or otherwise know how I can
> find more information.
>
> Thank you!
> Tom Brendlinger
> Senior Electrical Engineer
> Superpedestrian, Inc.
> 