TECHNET Archives

May 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Judy Brown <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Judy Brown <[log in to unmask]>
Date:
Fri, 4 May 2007 15:13:25 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (217 lines)
What is the % in screen test for solder paste on J-STD-005?

Regards,
        Judy Rae Brown
        Engineering & Quality Manager
        Smart Electronics
        phone 714-991-6500 ext. 225

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Friday, May 04, 2007 3:05 PM
To: [log in to unmask]
Subject: Re: [TN] Metallurgists, need assistance

Hi Dave,

I'm almost completely with you  and that was another reason I asked Inge
whether he happened to have a X-section of a bad lead.
:-)

Vlad


-----Original Message-----
From: [log in to unmask]
To: TechNet E-Mail Forum; Vladimir Igoshev
CC: [log in to unmask]
Sent: Fri May 04 17:55:51 2007
Subject: Re: [TN] Metallurgists, need assistance


Hi Vlad! If I am interpreting Inge's photo number 4 correctly [realize I
didn't get to see it on the SEM in person : - ) ], I see the nickel surfaces
which have no wetting of solder. Gold dissolves into solder at 100 uinches
per second (Bader data) there should be no gold on those surfaces. In
brittle interface fracture, I expect to see very few regions of nonwetting -
the failure is due to the poor properties of the Sn/Ni intermetallic (e.g I
get good wetting, its just not a strong interface). In cases of black pad, I
expect to see very few regions of good wetting, the nickel surface has been
corrupted such that I don't form the Sn/Ni intermetallic (e.g I get terrible
wetting and never form a good interface). Thus my comments for picture 4. 

Dave 



Vladimir Igoshev <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]> 

05/04/2007 04:12 PM 
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Vladimir Igoshev <[log in to unmask]>

	
To
	[log in to unmask] 
cc
	
Subject
	Re: [TN] Metalurgists, need assistance

	




Hi Dave,

I'm lost:-) how come you know there was no Au in the areas where we see Ni?

Brittlle Failed ENIG joints wqill have a similar "muddy" appearance

Regards,

Vladimir

-----Original Message-----
From: TechNet
To: [log in to unmask]
Sent: Fri May 04 16:45:09 2007
Subject: Re: [TN] Metalurgists, need assistance

Hi folks and thank you Steve for being "TechNet Picture Central"!  Sorry 
but just to warn everyone but I am going to use the "B" word shortly. Inge 
- take a close look at picture 4. As Werner pointed out the gold is 
non-wetting the nickel  in number of locations. What really jumped out at 
me is that "mud flat" appearance on some of the nickel surface regions - a 
"mud flat" appearance is a classic indication of black pad! I recommend 
you complete a cross-section to confirm that you have nickel grain 
boundary attack. 

But since it is Friday, go have a beer and worry about this on Monday!

Dave Hillman
Rockwell Collins
[log in to unmask]




Steve Gregory <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
05/04/2007 01:45 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Steve Gregory <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Metalurgists, need assistance






Hi Inge!

Got your pictures posted. Took me a bit, I was swapping our wave
solderpot from 63/37 to HMP. Done now. I'm getting quicker, I can do it
in 20-minutes now. Took me about 45-minutes when I first did it...

Anyways, here's the links:

http://stevezeva.homestead.com/files/Pic1.jpg
http://stevezeva.homestead.com/files/Pic2.jpg
http://stevezeva.homestead.com/files/Pic3.jpg
http://stevezeva.homestead.com/files/Pic4.jpg
http://stevezeva.homestead.com/files/Pic5.jpg
http://stevezeva.homestead.com/files/Pic6.jpg

-Steve-

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Friday, May 04, 2007 12:22 PM
To: [log in to unmask]
Subject: [TN] Metalurgists, need assistance

Have an issue with (randomly) lifted FPGA leads.
Pic 1: good joint after pull test
Pic 2: ditto but high magnification
Pic 3: "rotten" joint after pull test
Pic 4: ditto but high magnification
Pic 5: "rotten" cross section
Pic 6: ditto but high magnification

60Sn on ENIG, obviously a brittle region. Suspect Kirkendall voids, but
the pockets with zillions of Tin spheres (0.1 to 2 um in size) points at
insufficient peak temperature to make 100% melt and good solidifying. If
these little balls were Lead, I could understand, but they are Tin!
Never seen like. Any "quickhead" out there, need fast advice. 

Note: Pic 2, you can see the underlying board pad nickel as dark areas. 
An experienced analyst will hopefully recognize. No Phosphorous peaks!

My Friday headache.

Inge

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2