TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Joel Mearig <[log in to unmask]>
Date:
Tue, 4 Oct 2005 11:53:45 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lance Mayes <[log in to unmask]>
Subject:
From:
Lance Mayes <[log in to unmask]>
In-Reply-To:
<200510040909515.SM02952@cpujoel0224>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Hi Joel,

We have a similar set of headers that are hand soldered.  If this is an on
going process you might have your machinist build a fixture to hold the
pins in place
and the operators could then place the pins in the fixture and then the
boards on the fixture to solder them.
That's what we did for our problem.  One question, are the operators
soldering from the primary side or the secondary? We solder from the
secondary and the leads are much easier to solder.

Hope it works out for you.


                        P.  Lance Mayes CIT
                        Mfg. Trainer



Joel Mearig <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
10/04/2005 09:58 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Joel Mearig <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Hand Soldering Long Gold Pins






I have a number of assemblies that have long (0.5") connector pins that
must
be soldered in the board. The pins must remain gold so at the moment I am
trying to hand solder. This is a difficult process. The 0.100" spacing
makes
it difficult for my production personnel to solder without getting solder
on
the gold pins.



The connectors are double row and there are two beside one another
creating
a four pin bank of 0.100" spaced pins. Any thoughts on how I can improve
this process for the soldering personnel would be greatly appreciated.



Joel Mearig




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2