TECHNET Archives

April 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 26 Apr 2001 15:56:59 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (78 lines)
Hi, Jay Ju,

Are you talking about drill bits for PCB fabrication? If you are, I cannot
give you an inspection spec number, but major defects caused by incorrect
resharpening might include incorrect hole size and smearing of the hole
walls. Smearing will have to be cleaned up by reaming the holes prior to
plating or you will not achieve proper connection to inner layers, good
plating adhesion or even plating thickness.

If the bits are for a different application, please specify what it is.

Regards

Pete Duncan





                    Young Hwan Ju
                    <yhju@SIMMTEC        To:     [log in to unmask]
                    H.CO.KR>             cc:
                    Sent by:             Subject:     [TN] The standard bit inspection spec
                    TechNet
                    <[log in to unmask]
                    ORG>


                    04/26/01
                    02:08 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    yhju






Hi, all subscribers
In incoming inspection of  both new bit and resharpened bit, Can you make
me know the standard spec if anyone knows about that.
And I' would like to know the exclusive major defects caused by wrong bit
resharpening operation.

regards
Jay Ju

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2