TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=ISO-8859-1
X-To:
Date:
Mon, 8 Mar 2004 20:09:27 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Neil Flatter <[log in to unmask]>
Subject:
From:
Neil Flatter <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (18 lines)
We recently discovered a difference in procedure for extraction of salts for ion chromatography.  After soaking in IPA at 80°C for an hour, what should be done with the sample?  IPC-TM-650 2.3.28 doesn't specifically state that the PCB should soak in the IPA solution while cooling.  The extraction described in IPC-TM-650 2.3.25.1 requires that the PCB remain in the Kapak bag for half an hour while cooling.

Should the solution be shaken or otherwise agitated?  IPC-TR-583 would suggest that a static extraction is less efficient.  In the situation I'm in, these additions resulted in significantly different results.  The tests were requested in order to troubleshoot a solderability problem so the procedural question is more academic.  I'd just like to know if my methods are inconsistent with accepted practices.

Neil Flatter
Process Quality
TRW-Automotive

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2