TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 20 Jan 2010 09:25:13 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Nigel Burtt <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="windows-1252"
Content-Transfer-Encoding:
quoted-printable
From:
Nigel Burtt <[log in to unmask]>
Parts/Attachments:
text/plain (15 lines)
What PCB laminate material is this. Have seen in the past CAF like problem 
without the normal bias or time expected under certain conditions with one 
particular laminate and close via spacing like this. Like you, the symptoms 
initially pointed to a bad lot of ICs...

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2