TECHNET Archives

March 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Rich Olsen <[log in to unmask]>
Date:
Sat, 26 Mar 2005 17:28:00 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Type:
text/plain; charset=us-ascii
In-Reply-To:
6667
MIME-Version:
1.0
Comments:
DomainKeys? See http://antispam.yahoo.com/domainkeys
Parts/Attachments:
text/plain (47 lines)
Rich:  This contamination is not evident before applying photoresist?

If that is the case, it would suggest that the problem is photoresist "locking on" to the Copper.
Since the problem appears to be everywhere, it is probably caused by something before exposure.   Checked your lamination temperatures lately?  Changed the way you prepare the Copper for photoresist?  Changed electroless Copper chemistry?

Rudy Sedlak
RD Chemical Company

Rich Olsen <[log in to unmask]> wrote:
Hi,

Has anyone seen the following?
Surface contamination on top of electroless copper.
It prevents plating and subsequent etching.
It is both under the resist and in exposed areas during pattern plate and
etch.
It is small on the order of a mil or two, but there can be lots of it.
It seems to be in streaks, a spattered appearance.

thanks,
Rich

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------
Do you Yahoo!?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
 Make Yahoo! your home page

ATOM RSS1 RSS2