Hello Poh Kong,
I don't know if U already solved Ur problem (I do hope so) but Im still
going to share my excpirience regarding this issue...
I don't know what Ur process parameters are, but using soldering paste
that contains 2% silver , should solve Ur problem.
Wetting preferences (ENIG) are not as good as when using HASL finish but
are according IPC requirements...
Good luck!
Sasha
*************************************************************************
Sasha Miladinovic - Production Engineering
Amersham Biosciences, PCB Production, Umeå
Tel: +46 (0) 90 150 232
Fax: +46 (0) 90 138 372
E-mail: [log in to unmask]
*************************************************************************
Poh Kong Hui <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
2003-02-27 13:18
Please respond to "TechNet E-Mail Forum."; Please respond to Poh Kong Hui
To: [log in to unmask]
cc:
Subject: [TN] : Shining smooth solder joint on ENIG or Gold plating Board.
Hi Technetters,
Can someone advise me how to get a good smooth shining solder joint on the
ENIG board or board with gold plate SMT pads.
As I can understand that board subjected to reflow soldering, the solder
joint tends to look dull and not so smooth joint. But, is there any way to
get a good shining joint.
Thanks.
Poh
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|