TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Fri, 29 May 2009 16:20:27 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (138 lines)
........> How to improve on that? EASY, do not do T-shock in production 
[slow cooling rate after reflow to 1.5C/sec or less] and in testing go less 
severe or no T-shock at all.
>

Exactly what I pointed at in a recent message. The most dangerous moment for 
a electronic product is in the manufacturing line!  Good to hear guru W 
underline that.

Looking forward to the TN Friday light entertainments....have nothing myself 
at the moment

Inge






----- Original Message ----- 
From: "Werner Engelmaier /*" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 29, 2009 2:43 PM
Subject: Re: [TN] Looking for opinions on separation/delamination between 
copper land and dielectric material.


> Ni hao charming,
> That separation can occur during cooling from solder reflow [if too 
> fast=thermal shock] or in your T-shock test [would have been good to give 
> details.
> Your TSSOP leads are likely Alloy42 [=very stiff] and are very stubby 
> [=very stiff] with SAC-solder  [=very stiff].
> In T-shock it is NOT any CTE-mismatch that causes your problem [even 
> though it does not help, and may cause reliability problems with the 
> product], but the thermal gradients resulting from T-shock and causing 
> component/PCB warpage.
>
> How to improve on that? EASY, do not do T-shock in production [slow 
> cooling rate after reflow to 1.5C/sec or less] and in testing go less 
> severe or no T-shock at all.
>
> Werner
>
>
>
>
>
>
>
>
>
> -----Original Message-----
> From: Charming Chan <[log in to unmask]>
> To: [log in to unmask]
> Sent: Fri, 29 May 2009 4:45 am
> Subject: [TN] Looking for opinions on separation/delamination between 
> copper land and dielectric material.
>
>
>
>
>
>
>
>
>
>
> Hello All,
>
> Our guys ran a thermal shock test to verify solder joint reliability of a
> TSSOP component. The micro-section shows that there is a minor crack at 
> the
> toe side of the solder joint and a separation(delamination) between the
> copper land and the dielectric material.
>
> My question is,
>
> Where did the separation/delamination occur? PCB fab house, PCB assembly
> house, or thermal shock test?
>
> If the separation/delamination occurred at pcb fab house, then, what's the
> possible root cause gonna be?
>
> If the separation/delamination occurred at thermal shock test or pcb
> assembly house, then, is it caused by CTE mismatch between pcb base
> material, solder alloy, and gull-wing footprint? How to improve on that?
>
> Brain storm, and any input is appreciated.
> I will get the micro-section picture posted once I get it. Thank you all.
>
> Best Regards
> Charming Chan
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> ----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2