We monitor conveyor speed, imersion depth, parallelism and preheat. We do
this with a Wave Solder Optimizer on a daily basis.
>I have been asked by my Quality department to come up with four parameters to
>measure on the wave solder process. This can be put in a program for daily
>recording so that if something changes by a percentage, they can say that we
>need to evaluate the wave solder process. I have come up with two or three
>areas that need to be monitored, but am not sure if these are all critical.
>Does anyone have certain requirements that they track on a daily basis?
>
>Thanks!! (;)>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|