hi,
there are several around. what you don't want to do is use an rtv
adhesive/sealant that contains acetic anhydride/acetic acid.
this is by no means an endorsement, but dow corning 3145 is a candidate. on
the other hand, dow corning 732 is not one you'd want to use.
phil crepeau
-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Wednesday, October 14, 1998 11:42 AM
To: [log in to unmask]
Subject: [TN] RTV
Can anyone recommend manufacturer and type of RTV to hold down components
for communication application?
re,
Ken Patel
______________________________________________________
Ken Patel Phone: (408) 490-6804
1708 McCarthy Blvd. Fax: (408) 490-6859
Milpitas, CA 95035 Beeper: (888) 769-1808
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|