David,
You have requested so much in one e-mail. I have tested Minico, which is Ag
plated copper particles, on flex. I published a paper at SUR/FIN 99 on
Immersion Ag onto Cu to be used as flex circuits. When do you need all of
your questions answered?
Call me if you want me to do a brain dump on you. My boss says can spent
some time with people on the phone without a price tag.
Richard Haynes
609-497-4584
-----Original Message-----
From: [log in to unmask] <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Tuesday, November 17, 1998 5:00 PM
Subject: [TN] Conductive Carbon Ink / Silver Polymer Thick Film on Card Edge
Contacts
>I am looking for any and all information on the use of Conductive Carbon /
>Silver Ink Polymer Thick Film on PCB card edge contact tabs as a
>replacement for the gold plating, (gold fingers). I have information from
>Electra on the Electrodor material and from National Starch - Acheson on
>the Minico material. Does anyone have experience with use of these
>materials on PCB / PWB edge connector contact tabs? I am looking for
>electrical, mechanical, reliability, quality, cost, etc. characteristics
>comparing conductive PTF to the typical 30 micro-inch gold plating used.
>I appreciate and thank you for any information and leads.
>
>[log in to unmask] (512) 723-8481
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|