I would get a can or RAID and spray your incoming boards!
On another Wild Kingdom subject, did you know that on average a spider
is within 7 ft of every human on the planet!!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, November 16, 2004 3:41 PM
To: [log in to unmask]
Subject: [TN] Strange Soldermask Defect...
Hi All!
Well, I've run across some strange problems in my time, but this one is
a new one to me.
I was on the production floor just after lunch, close by one of our
final inspectors looking at something under her microscope, when I hear
her say; "What the heck is this?" then I hear this big; "EWWWWWW!" from
her...
"Steve! Steve! You gotta' look at this!" she says to me. I pull up a
chair and peer into the microscope, and I have to say, I've never, ever
seen this before.
Take a look at:
http://www.stevezeva.homestead.com/files/StrangeMaskDefect.jpg
and
http://www.stevezeva.homestead.com/files/StrangeMaskDefectCloseUp.jpg
What should I do? Should I send this to a lab or something? I don't know
what to tell my inspectors, much less explain this to our
customer...this really tops my list as one of the strangest defects I
have ever seen.
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|