We have manufactured thousands of boards with a mix of both ceramic and
plastic parts, mainly for military communications equipment. We use RMA
paste and an aqueous wash. We now place a much greater percentage of
plastic parts of course, because that is where the technology has migrated.
I have not yet had to deal with the issue of entrapped corrosive residues
in any of our product.

I don't buy the Rosin-bad, low residue-good argument. There are a lot of
good reasons to go with a low-residue process, but to just out of hand say
an RMA process is bad is not one of them IMO.

At 11:35 AM 12/16/98 -0800, you wrote:
>Season's Greets,
>
>A query (actually re-query) to those in the know on the usage of plastic
>microcircuits instead of ceramics.
>
>I have some component guys who have ruled that plastic parts can only be
>assembled on a no-clean flux line.  Anyone using a rosin (RMA) flux is
>dis-qualified from assembling for us.  I know the theory is that the
>microcracks formed at reflow temperatures will entrap corrosive residues,
>but I have trouble buying the NO-CLEAN GOOD, ROSIN-BAD generalization.
>
>Opinions?
>
>Ralph Vaughan
>Boeing-Atlanta
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
----

Jeffrey C. Guynn <[log in to unmask]> Phone: (219) 429-6345
Lead SMD Manufacturing Engineer        Fax: (219) 429-4688
Raytheon Systems Company M/S 25-31
1010 Production Road, Fort Wayne, IN 46808-4106

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2