I have worked before with the TM650 copper mirrors.
Has anyone ever worked with silver mirrors made in the same fashion? On a microscope slide.
I am looking for a source to make some for me.
Rich Kraszewski
Senior Staff Process Engineer- Plexus Corp.
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|
|
|