TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Bloomquist, Ken" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bloomquist, Ken
Date:
Tue, 4 Oct 2005 06:38:21 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
THANK YOU DOUG! You've made my day and possibly even my week. That's the
best laugh I've had in along time. You da man!

KennyB

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Tuesday, October 04, 2005 6:29 AM
To: [log in to unmask]
Subject: Re: [TN] Mixing Fluxes: Water Sol and Rosin

Well Ramon, just for you, I went and asked my Dad.

Based on his experience with flux and sweating copper pipes, you have to
rough up the copper pads on your board with 80 grit sandpaper, paint on
a
good heavy layer of flux with a brush on both the pad and component, and
make sure you hold the propane torch on the pad and lead a good long
time
to make sure it is up to temperature, then apply your wire solder, then
heat some more to make sure it wetted right.  Don't clean it and in a
little while the green patina will form on the copper.

Let me know how it works for you.

Doug Pauls
Some days I am just too funny for words......

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2