TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Stephen Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 15 Apr 2005 10:07:36 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (212 lines)
Hi Inge!

Got your pictures up! Go to: http://www.stevezeva.homestead.com and
look at "Too much gold 1", and "Too much gold 2"...

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX


|---------+--------------------------------->
|         |           "Ingemar Hernefjord   |
|         |           (KC/EMW)"             |
|         |           <ingemar.hernefjord@ER|
|         |           ICSSON.COM>           |
|         |           Sent by: TechNet      |
|         |           <[log in to unmask]>     |
|         |                                 |
|         |                                 |
|         |           04/15/2005 03:33 AM   |
|         |           Please respond to     |
|         |           TechNet E-Mail Forum; |
|         |           Please respond to     |
|         |           "Ingemar Hernefjord   |
|         |           (KC/EMW)"             |
|         |                                 |
|---------+--------------------------------->
  >--------------------------------------------------------------------------------------------------------------|
  |                                                                                                              |
  |       To:       [log in to unmask]                                                                              |
  |       cc:                                                                                                    |
  |       Subject:  Re: [TN] Tinning of Bipolar Transistor                                                       |
  >--------------------------------------------------------------------------------------------------------------|




Hi Ramon,
actually one thousand of an inch! Equal to 25 micrometers. When you
measured on various spots of the legs, the gold varied from 1 to nearly 25
micrometers. I'll post two pics for Steve's crowded galleria, one showing
the actual microwave device, the other a cross section of a leg with 10
micrometers of gold. The manufacturer of the hardware said, that it can be
a problem to get an even layer of gold on such devices. Nonsense...
Ingemar

-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: den 14 april 2005 16:51
To: TechNet E-Mail Forum; Ingemar Hernefjord (KC/EMW)
Subject: RE: [TN] Tinning of Bipolar Transistor



        Hi Ingemar:
                        What do you mean with a mil?  One thousand of an
inch or a millionth of an inch? My understanding has been the first one,
which is what I think you mean. Some books abbreviate millionth of an inch
as mil.
        Regards,
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Thursday, April 14, 2005 9:35 AM
To: [log in to unmask]
Subject: Re: [TN] Tinning of Bipolar Transistor


Steve,
warning: first of all, crossection one pc and have a look at the
gold thickness. We have a problem with degolding on a batch just now:
the ordinary dip-dip has to be prolonged because of too much gold. We
measured up to 1 mil of gold on some legs! And only a fraction of
that on another leg. Ideal is just a flash, if the nickel is good.
It's sometimes a problem to give correct plating to these tiny things.
In Chin...oops..

Ingemar Hernefjord
Ericsson Microwave Systems




Hi All!

We've got this Bipolar Microwave Transistor that I've just seen for
the first time, and I was asked if this part needs tinning because of
the gold plating.

I know what the J-STD says, but looking at the construction of the part,
I don't know if the part can withstand the heat of a tinning operation.

Take a look at "Bipolar Transistor" on my web page at:

http://www.stevezeva.homestead.com

I've tried to track down a datasheet, but can't seem to find one. The top
of the part is marked; "TRW 54601" and just below that, there's a "C86"
marked there.

The part may be very robust, and I have nothing to worry about. But
because this is the first time I've seen something like this, I thought I'd
ask the experts out there...

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2