TECHNET Archives

July 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Louis, Edwin @ CSE" <[log in to unmask]>
Date:
Thu, 12 Jul 2001 10:33:35 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Craig Hillman <[log in to unmask]>
Subject:
From:
Craig Hillman <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (50 lines)
Edwin,

The major concern over popcorning is delamination on top of the die. This
can lead to condensation, which can cause ECM between ball bonds or
corrosion of the bond pads. It can also cause shifting, which lead to
fatigue of the ball bonds and eventual liftoff.

I would strongly recommend not using these components.

Craig

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Louis, Edwin @ CSE
Sent: Thursday, July 12, 2001 9:30 AM
To: [log in to unmask]
Subject: [TN] PEMs


If one receives PEMs from the manufacturer which are supposedly dry and
handled correctly but are found to have internal delamination
by acoustic spectroscopy, whether this is an automatic sentence of
popcorning when the devices are put through convection reflow. Is there air
inside the part that can cause popcorning of a dry part when no outward
signs of delamination or popcorning is visible.Also,

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2