TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
JESS BAKER <[log in to unmask]>
Reply To:
"TechNet E-Mail Forum." <[log in to unmask]>, JESS BAKER" <[log in to unmask]>
Date:
Thu, 13 Aug 1998 08:57:46 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (50 lines)
High Phosphorous Nickle platings are difficult to impossible to solder to
without the use of acid fluxes. my recollection is that the low phospher
plating bath should be < 3-4% Phospher for successfull soldering ability.
Further given a low Phospher formulation Nickle oxides readily and again
will not be readily solderable with Organic acid fluxes. To prevent
re-oxidation of the Nickle the plater should thoroughly clean following
the Nickle bath and then immedialty overplate with 50-100 micro inches of
soft Gold I.e no brightners, hardners etc. The alternative is to hot
solder dip the Nickle to prevent re-oxidation of the lead.

since you are already having trouble intermittently sometime being able
to use a Rosin flux and sometime requiring a OA flux I assume the leads
already have a Gold finish as is the customary practice. solderability
problems are common with Gold finishes if not properly performed ,
causing the Gold to be porous and thus allowing the Nickle beneath it to
re-oxidize. The presence of organics due to poor cleaning will usually
evidence itself by forming pin-holes when soldered.

good luck

Jess

_____________________________________________________________________
You don't need to buy Internet access to use free Internet e-mail.
Get completely free e-mail from Juno at http://www.juno.com
Or call Juno at (800) 654-JUNO [654-5866]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2