TECHNET Archives

April 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Robert e. welch" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 24 Apr 2014 12:28:31 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (59 lines)
Thanks Mike.
Will get right on it!

Robert E. Welch
Senior Process Engineer
Moog Components Group

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Anil Kher
Sent: Thursday, April 24, 2014 5:13 AM
To: [log in to unmask]
Subject: Re: [TN] Thick gold plating

Besides hardness lot of other factors affect wearability. Surface smoothness, ductility and other components of the alloy matrix.
2% cobalt is good starting point .
Anil

-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]]
Sent: 23 April 2014 20:04
Subject: Re: Thick gold plating

Co.

"All professional skills are mastered by critiqued practice" - by Schon.
  Original Message
From: Victor Hernandez
Sent: Wednesday, April 23, 2014 9:55 AM
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Thick gold plating


Fellow TechNetters:

   Besides palladium, what other alloys can be added to gold/nickel to
improve hardness/wearability?   Is there an IPC dtandard?

Victor,

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2