I would say no - CAF is seen on packages that have good drilling,
lamination and glass wet-out.  Tight designs with pin placed close to
utilities should be reviewed closely for minimum spacings and the use of
CAF resistent materials (some other than FR4 also) may also be needed to
be evaluated.



Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com	



-----Original Message-----
From: Kane, Joseph E [mailto:[log in to unmask]] 
Sent: Wednesday, March 24, 2004 10:09 AM
To: [log in to unmask]
Subject: [TN] CAF And PWB Subsurface Imperfections


Does anything we know now about conductive anodic filaments indicate
that we should rethink acceptance of measles, or reconsider criteria for
delamination?

-Joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2