TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Guy M. Ramsey" <[log in to unmask]>
Date:
Mon, 19 Apr 2010 15:58:32 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Subject:
From:
Karen Tellefsen <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (76 lines)
Aqualine 6000 is halide-free, ORH0.  Must be washed, washable in hot DI
water.

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069



                                                                           
             "Guy M. Ramsey"                                               
             <gramsey@RDCIRCUI                                             
             TS.COM>                                                    To 
             Sent by: TechNet          [log in to unmask]                     
             <[log in to unmask]>                                          cc 
                                                                           
                                                                   Subject 
             04/19/2010 02:42          Re: [TN] Flux-Cored Wire Solder:    
             PM                        Halide / Halide-Free                
                                                                           
                                                                           
             Please respond to                                             
              TechNet E-Mail                                               
                   Forum                                                   
             <[log in to unmask]>                                             
             ; Please respond                                              
                    to                                                     
              "Guy M. Ramsey"                                              
             <gramsey@RDCIRCUI                                             
                  TS.COM>                                                  
                                                                           
                                                                           




Amtech makes a wire core solder with Halide free watersoluble flux. You
should
clean it but it cleans fairly easily. If you are looking to change your
cleaning
process, I recommend you look at it. We clean it with a spot steam cleaner.


If you are staying with alcohol you cannot use it.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2