TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Fri, 10 Dec 1999 11:19:41 +1100
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (149 lines)
Did . Yo're quite right, apart from the cost, it did not beat simple flash
as well (say 15umNi, 0.5umAu), on IPC-SM-785.
To this day i still owe Dave the report summary (some 7 months of cycling)
Did not see any improvement from (challenging) NiAu solderability/wetability
.
Still, keeping all smt corners and pth top pads wet,
never seen the black plague (must be doing something right)on floor . Few
outside .
But I have good fab fellows on bare cards, all in tight limits and fresh,
(reminds me, where's Earl ?).

As far as IMT's, the latest trends [LF]of exotics like NiPdAu soldered with
Ag alloys (NEMI)do puzzle me .
Tough joints , just the plasticity seems to be "bit" dry .
Well, Anatech just recalibrated my deep cycle toy, back to cracking caps .


cu jk                     pk


-----Original Message-----
From: joyce [mailto:[log in to unmask]]
Sent: Friday, 10 December 1999 10:02
To: [log in to unmask]
Subject: Re: [TN] Ni/Pd/Au


Does anyone did reliability test of the joint form with Ni/Pd/Au?  If my
memory serve me right, Pd and solder do form intermetallics relatively fast.
                                  jk
At 02:33 PM 12/9/99 -0700, you wrote:
>Larry,
>
>        You are absolutely correct.  However, in order for solder to make
>contact with Ni, it must first dissolve the Pd.
>
>        Several SMT solderability tests have used the technique of
depositing
>solder and measuring how far it spreads during reflow.  How far solder
>will spread is a function of the surface energy interface of the liquid,
>solid and gas, and the wetting angle.  By increasing the surface energy
>of the solid, the liquid can more easily wet that surface.  Without
>referencing a chart, I would guess that the energy interface of liquid
>Tin is better for Gold than Palladium because Gold dissolves into Tin
>faster.  Improving the solderability of Palladium by using flash gold
>was suggested by Elizabeth Benedetto in her article in SMT Feb 99 titled
>"Evaluation of Palladium Lead Plating".
>
>        Dave Hillman did do solderability testing and wire bonding on
Ni/Pd/Au
>and found that surface finish has very good wire bondability. (Published
>in SMI '96)  It is also corroborated by an NCMS consortium published in
>SMI '96. And ITRI reported the same results in IPC expo 97.
>
>        From the looks of the above stated articles, I guess I'm wrong
about
>the Au being used to improve solderability.  It sounds like the gold is
>for wirebonding.
>
>Ryan Grant
>
>>-----Original Message-----
>>From:  Larry Tawyea [SMTP:[log in to unmask]]
>>Sent:  Thursday, December 09, 1999 11:16 AM
>>To:    [log in to unmask]
>>Subject:       Re: [TN] Ni/Pd/Au
>>
>>In a message dated 12/8/99 4:02:17 PM Central Standard Time,
>>[log in to unmask] writes:
>>
>><<
>>         The gold is an attempt to improve the solderability of the
>>palladium. >>
>>Ryan,
>>
>>Unless I am totally missing something from your response,  the issue is
not
>>how long the solder is in contact with the Au or Pd but how long is the NI
in
>>contact with the solder.  I'm not trying to take issue with your response,
>>but I think the issue is what is the solderability of the Ni and how good
of
>>a solder joint have you made to the NI.
>>
>>Larry Tawyea
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>>text in
>>the body:
>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>To unsubscribe:   SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>>information.
>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>>847-509-9700 ext.5365
>>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2