Normally you use a core without copper when the number of prepregs used
between cores exceeds 4, to avoid slippage in the press and maintain good
thickness control.
regards
Dougal
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of SAHLI habib
Sent: 22 December 2008 14:40
To: [log in to unmask]
Subject: [TN] Multilayer construction
Hello,
Are there some rules which allow us to know when it's necessary to use a
blank material (core without copper) combined with prepreg?
What are the advantages and disadvantages if any?
Best regards.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Stevenage Circuits Limited.
Registered office: Caxton Way, Stevenage, Hertfordshire, SG1 2DF.
Registered in England under company number 1059497.
The views of the author may not necessarily represent those of
Stevenage Circuits Ltd.
This message may contain information and/or data that is confidential and legally privileged.
It is intended solely for the addressee(s) only.
If you are not the intended recipient you are notified that any use, publication, reproduction or dissemination is strictly prohibited.
In such an event, please contact the sender by return e-mail and
destroy this and all copies of this message and/or data.
Please be aware that the integrity of this email cannot be guaranteed,
as it is not a safe and secure medium for communication.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|