Hi, Kathy,
Rust is a very poor conductor, as anyone with a rusty car and wiring
trouble can testify. Corrosion on battery terminals can ruin a connection,
and where oxidisation is deliberate, such as in anodising of aluminium,
electrical conductivity is poor to non-existant, depending on the thickness
of the oxide layer.
Peter Duncan
Kathy Kuhlow
<Kathy@BTW-IN To: [log in to unmask]
C.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: Aero/ST Group)
TechNet Subject: [TN] Rusty
<[log in to unmask]
ORG>
11/30/01
01:55 AM
Please
respond to
"TechNet
E-Mail
Forum."
I was asked a question today and I can't seem to find the answer. I think
I know but I need more then a gut feel.
Is rust conductive, just a by product, or both? The materials we were
discussing are phosphorus, bronze, iron. Thanks in advance.
Kat
(See attached file: TEXT.htm)
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
|
|
|