TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Date:
Fri, 28 Jan 2005 14:47:11 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (105 lines)
Alistair

Following on from Brian's input, the purpose of this test standard is to
provide uniform and repeatable measurement results that may be compared from
site to site. It is intended to measure the robustness of the surface finish
under test, it is not intended to test your flux solderability. (It might be
used in this way, but that is not the intention) For that reason there are
now 3 standard fluxes:

SMNA
Actiec 2
Actiec 5

These are now actually explained in the latest standards releases.

Changing the test flux takes you outside the standard, so what would you
then be measuring?

Also, using some form of fume extraction is not as straightforward as you
might imagine. The measurement device is making minute force measurements
and any minor disturbance such as air flow and vibration will disturb your
tests.

The best solution I can give is to equip the operator with suitable
breathing apparatus.
--
Regards Graham Naisbitt

[log in to unmask]

Golf quote of the week: Columbus went around the world in 1492. That isn't a
lot of strokes when you consider the course.

Concoat Limited - Engineering Reliability in Electronics
A British Manufacturer

NEW WEB SITE: www.concoat.co.uk :NEW WEB SITE


Cell: 079 6858 2121
Office: +44 (0)1252 813706




On 28/1/05 8:57 am, "Alistair Murray" <[log in to unmask]> wrote:

> For health & safety requirements, I am seeking an alternative test flux
> to that prescribed for use in the solder testing of PCBs.
>
> This test flux comprises 25% colophony in alcohol.
>
> Colophony is classed as a Sensitizing Agent for Occupational Asthma.
>
> LEV is an option but I would prefer to use a safe flux of similar
> "activity".
>
>
>
> Does anyone know of a colophony-free flux of similar activity? I regret
> that I do not know the activity of the colophony flux (acid value?). Is
> there a way of comparing it with the activity of a synthetic flux?
>
>
>
> Many thanks in anticipation
>
>
>
>
>
> Alistair Murray
>
> Artetch Circuits Ltd
>
> UK
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2