Hello Rich,
We have used ASTM D2486 scrub resistance for wall paints to run scrub testing on stencil nano-coatings. This method requires a specific piece of equipment to do the testing. There is also a cross hatch adhesion test that involves cutting into the coating in a grid pattern and then tape testing to check adhesion. I am not sure about the ASTM number for this method.
Best regards,
Tony Lentz
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Richard Kraszewski
Sent: Wednesday, July 18, 2018 11:46 AM
To: [log in to unmask]
Subject: [TN] ASTM Spec for Coating Abrasion ??
Anyone aware of any ASTM method (or other industry method) that deals with handling/abrasion/marring of coatings that could lend itself to a nano coating evaluation?
Some nano coatings we are looking at are particularly soft and susceptibl.
Rich Kraszewski
Senior Staff Process Engineer
Plexus
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|
|
|